Ni-BaTiO3 multilayer ceramic capacitors (MLCC) have been aged at 121 °C and 100% Relative Humidity for 2,600 h. Raman and energy dispersive spectral measurements have been made on both aged and unaged samples. Raman spectra indicate the presence of a coating of substoichiometric SnO x (1 < x < 2) in the aged samples. Morphological and elemental changes occurring in the MLCC were examined by Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS). Preliminary, frequency dependent dielectric measurements indicate that ageing causes a substantial decrease (about 50%) of the capacitance, even if only surfaces are affected by the ageing phenomenon.

Raman investigation of the Ageing of Ni-BaTiO3 Multilayer Ceramic Capacitors

SCUOR, NICOLA;SERGO, VALTER
2008-01-01

Abstract

Ni-BaTiO3 multilayer ceramic capacitors (MLCC) have been aged at 121 °C and 100% Relative Humidity for 2,600 h. Raman and energy dispersive spectral measurements have been made on both aged and unaged samples. Raman spectra indicate the presence of a coating of substoichiometric SnO x (1 < x < 2) in the aged samples. Morphological and elemental changes occurring in the MLCC were examined by Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS). Preliminary, frequency dependent dielectric measurements indicate that ageing causes a substantial decrease (about 50%) of the capacitance, even if only surfaces are affected by the ageing phenomenon.
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11368/1705252
 Avviso

Registrazione in corso di verifica.
La registrazione di questo prodotto non è ancora stata validata in ArTS.

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 8
  • ???jsp.display-item.citation.isi??? ND
social impact