In order to investigate in detail the effects of dehydration and grinding on the mechanical shear behaviour of Ca-rich montmorillonite, a cycle of specific experimental shear deformation tests were performed on five typology of samples, preliminary controlled by thermal analysis (TG, DTA) and X-ray diffraction (XRD): (1) a natural Ca-montmorillonite containing about 5% of adsorbed water; (2) the same montmorillonite heated at 80 °C for 2 h to remove only the adsorbed water; (3) up to 250 °C for 2 h to remove also the interlayer water; (4) up to 340 °C for 2 h to complete the removal of interlayer water and start to introduce thermo-structural defects, and (5) the starting natural Ca-rich montmorillonite after hard ball-milling for 20 h to induce mechanical deformation and structural defects in the TOT layers. The five typologies of samples have been tested by a specifically designed and built shear box apparatus, under about 20 MPa condition of normal pressure. All samples, before and after the shear test, have been analysed by Optical Microscopy (OM), Scanning Electron Microscopy (SEM) and XRD. A theoretical mechanical analysis based on the Maxwell model is proposed to explain the τ(ε) and τ() shear behaviour of the effects of the different type of dehydration and deformation of the material, that was finally discussed in the context of the microstructural OM, SEM and XRD data.

Effects of dehydration and grinding on the mechanical shear behaviour of Ca-rich montmorillonite

Pini, G. A.;
2018-01-01

Abstract

In order to investigate in detail the effects of dehydration and grinding on the mechanical shear behaviour of Ca-rich montmorillonite, a cycle of specific experimental shear deformation tests were performed on five typology of samples, preliminary controlled by thermal analysis (TG, DTA) and X-ray diffraction (XRD): (1) a natural Ca-montmorillonite containing about 5% of adsorbed water; (2) the same montmorillonite heated at 80 °C for 2 h to remove only the adsorbed water; (3) up to 250 °C for 2 h to remove also the interlayer water; (4) up to 340 °C for 2 h to complete the removal of interlayer water and start to introduce thermo-structural defects, and (5) the starting natural Ca-rich montmorillonite after hard ball-milling for 20 h to induce mechanical deformation and structural defects in the TOT layers. The five typologies of samples have been tested by a specifically designed and built shear box apparatus, under about 20 MPa condition of normal pressure. All samples, before and after the shear test, have been analysed by Optical Microscopy (OM), Scanning Electron Microscopy (SEM) and XRD. A theoretical mechanical analysis based on the Maxwell model is proposed to explain the τ(ε) and τ() shear behaviour of the effects of the different type of dehydration and deformation of the material, that was finally discussed in the context of the microstructural OM, SEM and XRD data.
File in questo prodotto:
File Dimensione Formato  
Dellisanti et al 2018.pdf

Accesso chiuso

Descrizione: Articolo principale
Tipologia: Documento in Versione Editoriale
Licenza: Copyright Editore
Dimensione 2.26 MB
Formato Adobe PDF
2.26 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
2917734_Dellisanti et al 2018-PostPrint.pdf

accesso aperto

Descrizione: Post Print VQR3
Tipologia: Bozza finale post-referaggio (post-print)
Licenza: Digital Rights Management non definito
Dimensione 2.73 MB
Formato Adobe PDF
2.73 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11368/2917734
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 14
  • ???jsp.display-item.citation.isi??? 11
social impact